INCREASING THE WEAR RESISTANCE OF ROLLING BEARINGS BY APPLYING A CHROMIUM NITRIDE COATING
To determine the effect of Cr 2 N coating on the performance of rolling bearings, this article has studied the tribological and corrosion characteristics of thin-film coatings obtained by the MF method. The tribological characteristics of coatings were studied using the “ball on disk” scheme before and after Cr 2 N coatings were applied. As the counterbody was used a ball of SchCh15 (without coating). Analysis of cross-sections of wear tracks after testing indicates that there is virtually no wear after coating. The coated sample has a coefficient of friction of 0.14 0.17, i.e. it does not exceed the value of the coefficient of friction (<0.2) required for materials in dry friction pairs. The method of potentiometry was used to determine the corrosion of steel SchCh15 before and after applying a thin-film coating Cr2N.Corrosion tests were performed on a potentiostat-galvanostat P150, in a 4% solution of nitric acid (HNO3). The test results showed that after applying the Cr 2 N coating, the corrosion rate was 0.191 cm/year, i.e. half as much as that of uncoated steel SchCh15.
Сведения
- Журнал
- NNC RK Bulletin
- Опубликовано
- 2020 · № 1, С. 117-121
- Язык
- Английский
- ISSN
- 1729-7516 · 1729-7885
- Издатель
- Republican State Enterprise "National Nuclear Center of the Republic of Kazakhstan
- Аффилиации
- Sarsen Amanzholov East Kazakhstan State University
Shakarim State University of Semey