Wear of the piston of the drilling pump andbprolongation of its service life
This article examines the wear of the piston of a drilling pump and ways to extend its service life. The main mechanisms of wear, including abrasive, adhesive, corrosion and fatigue, as well as factors affecting its intensity, such as pressure, temperature, composition of drilling fluid and mechanical impact, are considered. A comparative analysis of various materials and protective coatings used to increase the wear resistance of pistons has been carried out. The study includes experimental tests of polyurethane pistons conducted on drilling rig No. 3, which is located on the Ayrankol area, well No. 278, and is operated by SBP KazMunayGas-Drilling LLP, the results of which showed their limited service life. Alternative solutions were considered, such as the use of coatings based on titanium nitride (TiN) and tungsten-carbide-cobalt (WC-Co), which demonstrated a significantly lower wear rate and a longer service life. For a comparative analysis, the wear resistance of pistons with different coatings under the operating conditions of a drilling pump is considered. The main indicator used is the wear rate (mm/hr). The wear rate of a drilling pump piston has been calculated for several coatings that are widely used in practice. A graph of the dependence of the wear of the piston of the drilling pump on the type of coating used is constructed. Based on the analysis, recommendations are proposed for optimizing the design of pistons, improving the composition of drilling mud and using modern coatings to increase the service life of piston systems of drilling pumps. The results obtained can be useful in upgrading pumping equipment and reducing operating costs in the oil and gas industry.
Сведения
- Журнал
- Neft i gaz
- Опубликовано
- 2025 · № 2, С. 62-73
- Язык
- Английский
- Цитирований
- 1
- ISSN
- 1562-2932 · 2708-0080
- Издатель
- Oil Research and Engineering Center of the National Engineering Academy of the Republic of Kazakhstan