PHASE RATIO AND CATALYTIC PROPERTIES OF COMPOSITES OF THE Al-SiC SYSTEM
The method of X-ray phase analysis established the synthesis of composites consisting of three phases: metallic aluminum, silicon carbide and silicon, by the method of electric spark dispersion of silicon carbide with aluminum in hexane and alcohol, and chemical analysis confirmed the presence of free carbon in these composites. The amount of aluminum in the composite synthesized in hexane is 1.8 times greater than silicon carbide, while in the composite synthesized in alcohol, on the contrary, there is 1.2 times more silicon carbide than aluminum. To study the catalytic properties of the synthesized composites, the reaction of decomposition of hydrogen peroxide in the liquid phase was chosen as a model. Composites of the Al-SiC system have catalytic activity in the reaction of hydrogen peroxide decomposition. The catalytic activity of the Al-SiC composite synthesized in alcohol is higher than the catalytic activity of the Al-SiC composite synthesized in hexane. The activation energy of the heterogeneous catalytic reaction of hydrogen peroxide decomposition is determined based on the temperature dependence of the rate of this reaction.
Сведения
- Опубликовано
- 2025 · Т. 10-895, № 2/2, С. 30-37
- Язык
- Английский
- ISSN
- 1694-7851 · 1694-8505
- Издатель
- Kyrgyz State University named after I. Arabaev
- Аффилиации
- Kyrgyz state university named after I. Arabaev