Bulletin of the Karaganda university - Physics, 2021, т. 102, № 2, с. 6-13
Research of annealing influence on the hardness of detonation coatings from aluminum oxide
Аннотация · Abstract
The article examines the effect of annealing on the structure and properties of alumina-based coatings obtained by detonation spraying. Coated samples were kept separately at temperatures of 500, 700, 800 and 1200 °C at a pressure of 3.6*10-4 Pa for more than 1 hour. It was found that the microhardness of coatings made of alumina increases by 15-30 % after annealing depending on annealing temperature. The results of nanoindentation show that at 1200 °C the nanohardness of coatings after annealing increases by almost 100%. Aluminum oxide coating is characterized by high strength and density of the coating before and afterannealing, and slight porosity. Results of X-ray analysis showed that the alumina powder consists of α-Al2O3 lattice, and after detonation injection coating cubes are converted into a semi-γ-cubic lattice. It was found that during the annealing of the coating at 1200 °C all cells of γ-phase completely transit to the α-phase. It was found that the increase in hardness after annealing of alumina coating at 500, 700, 800 and 1200 °C is associated with an increase in volume fraction of α-Al2O3 phase.
Сведения · Details
- DOI 10.31489/2021ph2/6-13
- Журнал · Journal Bulletin of the Karaganda university - Physics
- Язык · Language английский
- Цитирования (Crossref) · Citations 0